MONEL 400
NiCu32Fe1.5Mn
Ni63 min Cu28-34 Fe1-2.5 Mn0-2
| Chemical composition |
|---|
Cu28-34
Ni63 min
Pb0.009 max
Fe1-2.5
Mn2 max
Si0.5 max
S0.02 max
Al0.5 max
C0.15 max
Ti0.3 max
| Alloy name | |
|---|---|
| RLSA no. | 430 |
| EN standard | |
| DIN standard | 2.4360 |
| UNS no.* | N04400 |
*Unified Numbering System (USA)
Characteristics and main uses
| Physical properties | Units | |
|---|---|---|
| Density (20°C) | 8,83 | Kg/dm³ |
| Melting point | 1300-1350 | °C |
| Longitudinal elasticity modulus | 179 | GPa |
| Thermal conductivity | W/m·K | |
| Electrical conductivity | 3,6 | m/Ω·mm² |
| Electrical resistivity | 55 | µΩ·m |
| Linear expansion Coefficient | 13,9 | 10⁻⁶·K⁻¹ |
| IACS (International Annealed Copper Standard) | % | |
| Poisson's ratio |
| Capabilities | |
|---|---|
| Corrosion resistance | 4 |
| Hot deformation | |
| Cold deformation | |
| Electrodepositing | |
| Diamond cutting | |
| Nitriding | |
| Mechanical polishing | |
| Welding without filler | |
| Brazing |
1 poor | 2 average | 3 good | 4 very good | - no info